Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Ultramid® A3EG3 - PA66-GF15 - BASF

Material Data Center offers the following functions for Ultramid® A3EG3:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Ultramid A datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Caracteristicas de procesamiento y fisicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de fluidez volumétrico, MVR 70 / * cm³/10min ISO 1133
Temperatura 275 / * °C -
Carga 5 / * kg -
ASTM Data
Contracción posterior al moldeo, paralelo 0.0055 mm/mm ASTM D 955
Propiedades mecánicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Módulo de tracción 6000 / 4500 MPa ISO 527
Esfuerzo de fluencia 130 / 85 MPa ISO 527
Alarg. nominal a rotura 3 / 10 % ISO 527
Módulo de flexión, 23°C 5500 / 4000 MPa ISO 178
Módulo de plastodeformación, 1000h * / 2500 MPa ISO 899-1
Resistencia al impacto Charpy, +23°C 45 / 70 kJ/m² ISO 179/1eU
Resistencia al impacto Charpy, -30°C 43 / - kJ/m² ISO 179/1eU
Resistencia al impacto Charpy c/entalla, +23°C 8 / 11 kJ/m² ISO 179/1eA
Resistencia al impacto Charpy c/entalla, -30°C 7 / - kJ/m² ISO 179/1eA
Resistencia al impacto Izod con entalla, +23°C 5.5 / 6.5 kJ/m² ISO 180/1A
Ball indentation hardness 200 / 150 MPa ISO 2039-1
ASTM Data
Esfuerzo de fractura a tracción 114 / - MPa ASTM D 638
Alargamiento a la rotura 3 / - % ASTM D 638
Módulo de flexión 5170 / - MPa ASTM D 790
Resistencia al impacto Izod con entalla, 1/8 in 59 / - J/m ASTM D 256
Resistencia al impacto Izod con entalla, baja temperatura 53 / - J/m ASTM D 256
Temperatura -40 °C -
Propiedades térmicasSeco / CondUnidadesMétodo de ensayo
ISO Data
Temperatura de fusión, 10°C/min 260 / * °C ISO 11357-1/-3
Estabilidad al calor, 1.80 MPa 250 / * °C ISO 75-1/-2
Estabilidad al calor, 0.45 MPa 250 / * °C ISO 75-1/-2
Coef.de expansión térmica lineal, paralelo 32 / * E-6/K ISO 11359-1/-2
Coef.de expansión térmica lineal, normal 75 / * E-6/K ISO 11359-1/-2
Combustibilidad a 1.5mm esp. nom. HB / * class IEC 60695-11-10
Espesores de probeta 1.6 / * mm -
ASTM Data
Estabilidad al calor @ 66 psi 250 °C ASTM D 648
Estabilidad al calor @ 264 psi 250 °C ASTM D 648
Temperatura de fusión 260 °C ASTM D 3418
Propiedades eléctricasSeco / CondUnidadesMétodo de ensayo
ISO Data
Constante dieléctrica, 1MHz 3.5 / 5.5 - IEC 62631-2-1
Factor de pérdidas dieléctricas, 1MHz 140 / 1600 E-4 IEC 62631-2-1
Resistividad volumétrica específica 1E13 / 1E10 Ohm*m IEC 62631-3-1
Resistividad superficial específica * / 1E10 Ohm IEC 62631-3-2
Indice comparativo de linea de fuga 550 / - - IEC 60112
ASTM Data
Resistividad volumétrica 1E13 / - Ohm*cm ASTM D 257
Otras propiedadesSeco / CondUnidadesMétodo de ensayo
Absorción de agua 7 / * % Sim. to ISO 62
Absorción de humedad 2.2 / * % Sim. to ISO 62
Densidad 1230 / - kg/m³ ISO 1183
Absorción de agua, equilibrio 7 % ASTM D 570
Densidad 1240 kg/m³ ASTM D 792
Propiedades específicas del materialSeco / CondUnidadesMétodo de ensayo
ISO Data
Indice de viscosidad 145 / * cm³/g ISO 307, 1157, 1628
Características
Procesamiento y forma de entrega
Moldeo por inyección, Otros tipos de extrusión
Forma de suministro
Sémola, Color natural
Applicaciones
Automotriz, Electrica
Disponibilidad regional
Norteamérica, Asia Pacifico
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.